1 / 5
| Still deciding? Get samples of $ ! US$ 20/Piece Request Sample |
Process Features: The metallurgical combination of the two materials is achieved through the liquid fusion process of the two metals, combining the excellent wear resistance of high-chromium cast iron and the good toughness of alloy steel. The striking part uses high-chromium cast iron (Cr20~30%), while the handle uses high-toughness alloy steel.
| Category | Impact Toughness (AK J/cm²) | Hardness (HRC) | Microstructure | Performance / Service Life |
|---|---|---|---|---|
| Cr15 | ≥8 | ≥60 | M+M7C3+M23C6+A | Mills < 3m, 3-5 years life |
| Cr20 | ≥8 | ≥60 | M+M7C3+M23C6+A | Mills > 3m, 3-8 years life |
| Cr26 | ≥8 | ≥60 | M+M7C3+M23C6+A | Mills > 4m, 5-10 years life |






Xingli Industrial Ceramics